What to notice
- The ram moves slowly, but the tube leaves about 10 times faster. The tube's cross-section is about a tenth of the billet's, and the volume of metal does not change.
- The squares in the billet are squeezed together in the cone and stretched into long, thin strips in the tube.
- The metal divides round the legs of the spider and joins again behind them, under high pressure, before it leaves the die. Each join leaves a weld line along the tube.
- Welding inside the die works well only for aluminium and some of its alloys, and no lubricant can be used (Kalpakjian and Schmid, p. 423).
- At the end of the stroke a short piece of billet, the butt, is left in the container and is cut off.
Schematic, not to scale. Arranged as in Kalpakjian and Schmid, Fig. 15.8(b). See also the static model of a spider die.